Components

PerformCoat Components

DLC (amorphous)CrN + DLCCrN Me-DLCHard-Carbon
Coating materialA-C:HCrN + a-C:H:WCrNA-C:H:W (WC/C)Ta-C
Hardness (HV0.05)2,5002,5002,3001,6506,000
Typical thickness (μm)1-51-51-301-4< 2
Increasing of roughness Ra (μm)0.020.020.020.020.01
Friction coefficient against steel0.150.150.40.150.05
Max operating temperature (°C)350350750300400
TechnologyRF/dc pulsedPVD+DC pulsed /
PVD + RF
PVDPVD+DC pulsedarc